pretty good job. option we use is to build up the grate IN the combine, then hardsurface the top layer and using a straight edge grind level. This will handle hours of service. Just a note here, when we use steep pitch helicals over the THRESHER side transistion into the sep std helicals and add the helical extention the RH wear factor us lessed by 80% or more. Also less HP is used. Eliminating the double pass threshing is a big fuel savings as well.